  • Yener, Tuba; Doleker, Kadir Mert; Erdogan, Azmi; Oge, Mecit; Er, Yusuf; Karaoglanli, Abdullah Cahit; Zeytin, Sakin (2022)
    In this study, an aluminide coating was applied to the surface of the Inconel 600 (IN600) superalloy to improve the high-temperature oxidation and wear resistance. The low-temperature aluminizing process was carried out ...